z-logo
open-access-imgOpen Access
STUDI EXPERIMEN KUAT TEKAN BETON DENGAN MEMANFAATKAN LIMBAH KERAMIK DAN BATA MERAH
Author(s) -
Satria Febby Romaadhoni,
Ahmad Ridwan,
Sigit Winarto,
Agata Iwan Candra
Publication year - 2019
Publication title -
jurnal manajemen teknologi dan teknik sipil
Language(s) - English
Resource type - Journals
ISSN - 2621-7686
DOI - 10.30737/jurmateks.v2i1.394
Subject(s) - brick , compressive strength , ceramic , materials science , flexural strength , composite material
Normal concrete sample (1) has a compressive strength of 222.22 kg/cm, normal concrete (2) has a compressive strength of 242.933 kg/cm, concrete using a mixture of ceramic 21% and red brick 7% sample (1) has a compressive strength of 177.911 kg/cm, concrete using a mixture of 21% Ceramics and red brick 7% sample (2) has a compressive strength of 189.777 kg/cm, concrete using a mixture of 10% Ceramics and red brick 4% sample (1) has a compressive strength of 204.667 kg/cm, concrete which uses a mixture of 10% Ceramics and red brick 4% sample (2) has a compressive strength of 137,333 kg/cm. It shows that the compressive strength of concrete decreases from increasing the volume of ceramics because the ceramic surface cannot bind perfectly. The highest K-204,667 with a mixture of 10% ceramics and 4% red brick and 28-day-old concrete, while to reach the K-250, is very far away. Of the 6 samples, the average reached K-195,807.Sampel beton normal (1) memiliki kuat tekan 222,22 kg / cm, beton normal (2) memiliki kuat tekan 242.933 kg / cm, sampel beton menggunakan campuran keramik 21% dan bata merah sampel 7% (1) memiliki kuat tekan 177.911 kg / cm, sampel beton menggunakan campuran keramik 21% dan bata merah 7% (2) memiliki kuat tekan 189.777 kg / cm, sampel beton campuran 10% Keramik dan bata merah 4% (1) kuat tekan 204.667 kg / cm, sampel beton yang menggunakan campuran Keramik 10% dan sampel bata merah 4% (2) memiliki kuat tekan 137.333 kg / cm. Ini menunjukkan bahwa Kuat tekan beton semakin berkurang dari bertambahnya volume keramik, karena permukaan keramik tidak bisa mengikat dengan sempurna. K-204.667 tertinggi dengan campuran 10% keramik dan 4% bata merah serta beton berumur 28 hari, sedangkan untuk mencapai K-250 sangat jauh jauh. Dari 6 sampel tersebut rata-rata mencapai K-195.807.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.