DEGRADASI METHYLENE BLUE MENGGUNAKAN KATALIS ZnO-PEG DENGAN METODE FOTOSONOLISIS
Author(s) -
Hary Sanjaya
Publication year - 2017
Publication title -
eksakta
Language(s) - English
Resource type - Journals
eISSN - 2549-7464
pISSN - 1411-3724
DOI - 10.24036/eksakta/vol18-iss02/45
Subject(s) - methylene blue , absorbance , nuclear chemistry , polyethylene glycol , peg ratio , fourier transform infrared spectroscopy , wurtzite crystal structure , chemistry , degradation (telecommunications) , analytical chemistry (journal) , zinc , photocatalysis , chromatography , catalysis , organic chemistry , chemical engineering , telecommunications , finance , computer science , engineering , economics
Study about degradation of methylene blue using photosonolysis method has been done. This research aims to investigate  effect of variation radiation times, pH, and concentrations doping PEG (polyethylene glycol). The absorbance of samples was measured by a UV-Vis spectrophotometer. The result showed maximum time of irradiation to degradate methylene blue at 120 minutes, with  percentage degradation is 94.55%. The effect of pH showed maximum pH at 7 with  percentage degradation is 96,83%. Meanwhile, the effect of variation concentration doping PEG showed maximum result at ZnO-PEG 15%, with percentage degradation is 87,12%. Sample was characterization by  XRD, FTIR and UV-DRS. The XRD pattern showed  wurtzite (hexagonal) structure and has crystal size of 47-88 nm. FTIR spectrum showed that 425,33 cm-1  vibration strain for Zn-O. Analysis UV-DRS obtained band gap value is  3.19 eV.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here