Термооптические и диэлектрические исследования сегнетоэлектрической фазы, индуцированной кальцием, в виртуальном сегнетоэлектрике SrTiO-=SUB=-3-=/SUB=-
Author(s) -
P. A. Markovin,
В. А. Трепаков,
M. E. Guzhva,
A. Dejneka,
Aleksey G. Razdobarin,
О.Е. Квятковский
Publication year - 2018
Publication title -
fizika tverdogo tela
Language(s) - English
Resource type - Journals
eISSN - 1726-7498
pISSN - 0367-3294
DOI - 10.21883/ftt.2018.09.46393.081
Subject(s) - ferroelectricity , dielectric , refractive index , condensed matter physics , polarization (electrochemistry) , birefringence , permittivity , atmospheric temperature range , materials science , analytical chemistry (journal) , optics , chemistry , physics , thermodynamics , optoelectronics , chromatography
We have examined temperature changes of the light refraction, birefringence, dielectric permittivity, and dielectric hysteresis loops in Sr_1 – x Ca_ x TiO_3 single crystals with x = 0.014 (SCT-1.4). The dielectric properties of Sr_1 – x Ca_ x TiO_3 with x = 0.007 (SCT-0.7) have been studied. We have performed ab initio calculations of equilibrium structures and total energies for three low-temperature phases of SrTiO_3 and CaTiO_3, based on which we have determined an expected symmetry of the ground state of their solid solution and spontaneous polarization directions in a calcium-induced ferroelectric phase in Sr_1 – x Ca_ x TiO_3. In SCT-1.4, we have separated a spontaneous contribution to the light refraction, which arises due to the spontaneous electrooptical effect caused by the spontaneous polarization and its fluctuations. From the spontaneous contribution to the light refraction, based on a previously developed our phenological approach, we have quantitatively determined for the first time the values and temperature dependences of root-mean-square fluctuations of the order parameter—the polarization P _sh = 〈 P _fl ^2 〉^1/2(short-range, local polar order) in the ferroelectric phase. From optical and dielectric measurements in SCT-1.4, the average value of spontaneous polarization P _ s (the contribution from the long-range order) has been determined. We have estimated the values of P _sh and P _ s , which characterize the short- and long-range orders in the ferroelectric phase of SCT-0.7. Separate determination of the values and temperature dependences of P _ s and P _sh (which considerably exceeds the value of P _ s in the ordered phase) has allowed us to reveal on a quantitative level new particular features of the formation of the induced polar phase in Sr_1 – x Ca_ x TiO_3.