MECHANICAL BEHAVIOR AND MICROSTRUCTURE EVOLUTION OF THE Ti-3Al-5Mo-4.5V ALLOY AT AN ELEVATED DEFORMATION TEMPERATURE
Author(s) -
Menglan Shen,
Yuanming Huo,
Tao He,
Yong Xue,
Ke Duan,
Wanbo Yang
Publication year - 2021
Publication title -
materiali in tehnologije
Language(s) - English
Resource type - Journals
eISSN - 1580-3414
pISSN - 1580-2949
DOI - 10.17222/mit.2020.088
Subject(s) - materials science , microstructure , deformation (meteorology) , softening , alloy , strain rate , atmospheric temperature range , deformation mechanism , metallurgy , titanium alloy , composite material , compression (physics) , thermodynamics , physics
A high-performance titanium alloy requires a fine and homogenous microstructure. The rational deformation process parameters of the Ti-3Al-5Mo-4.5V (TC16) titanium alloy can contribute to achieving this important microstructure. Hot-compression experiments were performed at temperatures in the range 100–800 °C and at strain rates of 0.1 s–1 to 10.0 s–1. The effects of deformation temperatures and deformation rates on the mechanical behaviour and microstructure evolution were analysed and discussed. The softening mechanism of the Ti-3Al-5Mo-4.5V alloy at an elevated deformation temperature was revealed. Experimental results showed that 500 °C is the critical deformation temperature to distinguish the warm-deformation region of 100–400 °C and the hot-deformation region of 500–800 °C. The softening mechanism is dominated by -phase spheroidization in the temperature range 100–400 °C with a higher strain rate of 10.0 s–1. The softening mechanism is dominated by a local temperature rise in the temperature range 500–800 °C with a lower strain rate of 0.1 s–1.