Synthesis of Blue‐Green Phosphors Sr4Si3O8Cl4:Eu2+ by Gel‐Combustion Method and Their Luminescent Properties
Author(s) -
Yongqing Zhai,
Lili Wang,
Juan Chen,
Feng Shihua
Publication year - 2012
Publication title -
journal of chemistry
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.436
H-Index - 50
eISSN - 2090-9063
pISSN - 2090-9071
DOI - 10.1155/2013/683404
Subject(s) - phosphor , orthorhombic crystal system , chemistry , luminescence , analytical chemistry (journal) , calcination , doping , emission spectrum , crystallography , crystal structure , spectral line , optics , materials science , catalysis , physics , optoelectronics , biochemistry , chromatography , astronomy
Sr4Si3O8Cl4:Eu2+ blue-green phosphors were synthesized by the gel-combustion method. The as-synthesized phosphors were analyzed and characterized by X-ray diffraction and fluorescence spectrophotometer. The results indicate that orthorhombic phase Sr4Si3O8Cl4:Eu2+ has been formed after the precursor calcined at 900°C reductive temperature. The excitation spectrum of Sr4Si3O8Cl4:Eu2+ is a broad band in the range of 250 ~ 450 nm and the main peak at 324 nm. The emission spectrum is also a broad band with the main emission peak at about 484 nm, which is ascribed to the typical 4f5d1 to 4f7 transition of Eu2+. Moreover, the effects of the concentration of Eu2+, the reductive temperature, and the doping amount of Mg2+ on luminescent properties were discussed
Accelerating Research
Robert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom
Address
John Eccles HouseRobert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom