Surface Plasmon Resonance Biosensor Performance Analysis on 2D Material Based on Graphene and Transition Metal Dichalcogenides
Author(s) -
Devi Taufiq Nurrohman,
Nan Fu Chiu
Publication year - 2020
Publication title -
ecs journal of solid state science and technology
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.488
H-Index - 51
eISSN - 2162-8777
pISSN - 2162-8769
DOI - 10.1149/2162-8777/abb419
Subject(s) - graphene , biosensor , materials science , surface plasmon resonance , nanotechnology , monolayer , tungsten diselenide , characterization (materials science) , transition metal , oxide , sensitivity (control systems) , plasmon , surface plasmon , optoelectronics , nanoparticle , electronic engineering , chemistry , engineering , biochemistry , metallurgy , catalysis
Since graphene was first isolated in 2004, research related to graphene-based 2D material for surface plasmon resonance (SPR) biosensor applications has increased. Recently, other types of 2D materials such as Transition Metal Dichalcogenides have also been investigated. This 2D material has exceptional optical and electronic properties and can be utilized to improve the performance of biosensors. The performance of SPR biosensors can be determined based on their sensitivity and detection accuracy (DA). To find out the sensitivity and DA, simulation approach can be done. In this paper, we perform SPR simulations on monolayer and multilayer structures of 2D material, namely graphene, graphene oxide, molibdenum disulfida, and tungsten diselenide. In addition, we also investigated the sensitivity and DA of SPR biosensors on hybrid structures. The results obtained indicate that the use of 2D material can increase the sensitivity of the SPR up to 5 times when compared to conventional structures. Of the four types of 2D material investigated, GO is the material with the best accuracy. If the SPR biosensor performance is determined based on the FOM value, the best performance is owned by the GO-based SPR structure with a sensitivity of 151.87 deg/RIU and DA 0.22 deg-1.