An In Vitro Evaluation of Human Enamel Surfaces Subjected to Erosive Challenge After Bleaching
Author(s) -
Vasconcelos Maria,
FonsecaGonçalves Andréa,
de França adílis Kalina Alexandria,
de Medeiros Urubatan Vieira,
Maia Lucianne Cople,
Queiroz Celso Silva
Publication year - 2016
Publication title -
journal of esthetic and restorative dentistry
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.919
H-Index - 60
eISSN - 1708-8240
pISSN - 1496-4155
DOI - 10.1111/jerd.12277
Subject(s) - enamel paint , in vitro , dentistry , dental enamel , materials science , chemistry , composite material , medicine , biochemistry
Objectives This study aimed to evaluate whether tooth enamel bleached with hydrogen peroxide (H 2 O 2 ) is more susceptible to erosion when compared with unbleached tooth enamel; and whether the presence of calcium (Ca) in the bleaching gel influenced this process. Materials and Methods Enamel blocks were prepared from human molars, and submitted to surface microhardness analysis (baseline). Blocks were prepared and randomly divided into four treatment groups ( n = 20): G1 and G2—bleached with 7.5% H 2 O 2 , with and without Ca, respectively; G3 and G4—bleached with 35% H 2 O 2 , with and without Ca, respectively. After bleaching, these groups were submitted to an erosive challenge with 1% citric acid. G5 and G6 ( n = 20, each) were the negative (without bleaching) and positive controls (without bleaching, but with erosion), respectively. The percentage of surface hardness loss (%SHL), the 3D non‐contact profilometry and Scanning Electron Microscopy (SEM) analyses were performed. Results G2 showed the highest %SHL after bleaching. G1 presented the lowest %SHL in comparison with G2, G3, G4, and G6 after erosion ( p < 0.05), which was confirmed only by the SEM analysis. Conclusion It is suggested that low concentration of H 2 O 2 with calcium can be recommended for at‐home bleaching agents, which may avoid the mineral loss of bleached enamel after an erosive challenge. Clinical Significance Low concentration of H 2 0 2 with calcium can be recommended for at‐home bleaching agents, which may avoid the mineral loss of bleached enamel after an erosive challenge. (J Esthet Restor Dent 29:128–136, 2017)