The edge chipping test was used to measure the fracture resistance of alumina/alumina‐zirconia laminated structures. Tailored, symmetrical laminated structures were prepared with a variety of layer thickness. The laminates had a significantly greater edge chipping resistance. Laminates with thin layers were just as effective in impeding edge chips as laminates with thick layers.