DOI - 10.1111/j.1744-7402.2012.02853.x
Subject(s) - materials science , silicon nitride , ceramic , slurry , composite material , fabrication , joint (building) , microstructure , coating , nitride , silicon , metallurgy , layer (electronics) , structural engineering , medicine , alternative medicine , pathology , engineering
This study demonstrated that a long silicon nitride pipe of several meters with adequately strong joints can be fabricated by a local‐heating joining technique. Commercially available silicon nitride ceramic pipes sintered with Y 2 O 3 and A l 2 O 3 additives were used for parent material, and powder slurry of S i 3 N 4 ‐ Y 2 O 3 ‐ A l 2 O 3 ‐ S i O 2 system was brush‐coated on the rough or uneven end faces of the pipes. Joining was carried out by locally heating the joint region at different temperatures from 1500°C to 1650°C for 1 h with a mechanical pressure of 5 MP a in N 2 flow; using a horizontal electrical furnace specially designed for this experiment. The silicon nitride pipe 3‐m long was successfully fabricated without voids or cracks in the joint region, and the microstructure of the joint region was similar to that of the parent one. The joint strength was examined in flexure using specimens cut from the joined pipes, and those joined at 1600°C and 1650°C indicated the highest strength of about 680 MP a, which was almost the same as that of the parent material. This study also indicated that the slurry brush‐coating technique is advantageous to easily joining ceramic pipes with rough or uneven end faces, which is essentially important for practical use.