Room‐Temperature Mechanical Behavior of Fiber‐Reinforced Ceramic‐Matrix Composites
Author(s) -
Mah T.,
Mendiratta M. G.,
Katz A. P.,
Ruh R.,
Mazdiyasni K. S.
Publication year - 1985
Publication title -
journal of the american ceramic society
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.9
H-Index - 196
eISSN - 1551-2916
pISSN - 0002-7820
DOI - 10.1111/j.1151-2916.1985.tb15261.x
Subject(s) - composite material , materials science , ceramic matrix composite , flexural strength , tension (geology) , ultimate tensile strength , ceramic , fiber , stress (linguistics) , matrix (chemical analysis) , linguistics , philosophy
Ceramic‐matrix composites reinforced with SiC fibers were tested at room temperature both in, flexural and tensile configurations. The stress‐strain behavior for composites tested in tension was correlated with progressive microcracking and failure processes. Significant differences between failure modes in tension and flexure were observed.