Study of the main metallurgical characteristics of iron ore raw materials (sinter and pellets)
Author(s) -
Galina Yu. Vitkina,
А. Н. Дмитриев,
Roman V. Alektorov
Publication year - 2020
Publication title -
iop conference series. materials science and engineering
Language(s) - English
Resource type - Journals
eISSN - 1757-899X
pISSN - 1757-8981
DOI - 10.1088/1757-899x/966/1/012061
Subject(s) - blast furnace , metallurgy , materials science , smelting , coke , raw material , pellets , iron ore , pelletizing , sintering , softening point , composite material , chemistry , organic chemistry
The paper presents the results of studies of the chemical, phase composition and metallurgical characteristics of titanomagnetite sinter. The iron ore used in blast furnaces of JSC ‘EVRAZ NTMK’ is titanomagnetite sinter obtained from ores of the Gusevogorsky deposit. Samples of sinter with different basicities as well as with addition of binding polymers in the amount of 300 and 500 g per ton of sinter were investigated. The results of industrial tests of the production and blast furnace smelting of sinter with different basicities and additives of binding polymers are presented on the example of the operation of blast furnaces no. 5 and 6 of JSC ‘EVRAZ NTMK’. It was shown that an increase in the basicity of the sinter from 2.1 to 2.4 and the introduction of a polymer binder (in the amount of 500 g per ton of sinter) positively affect the complex of sinter metallurgical characteristics – durability after reduction, reducibility, softening and melting temperatures, and also decrease the coke rate in blast furnace smelting by 1.0–1.2%.