Mechanical and physical properties of bottom ash/fly ash geopolymer for pavement brick application
Author(s) -
Wan Mastura Wan Ibrahim,
Mohd Mustafa Al Bakri Abdullah,
Romisuhani Ahmad,
Muhammad Faheem Mohd Tahir,
Nurul Aida Mohd Mortar,
Muhammad Amirul Aziem Noor Azli
Publication year - 2020
Publication title -
iop conference series. materials science and engineering
Language(s) - English
Resource type - Journals
eISSN - 1757-899X
pISSN - 1757-8981
DOI - 10.1088/1757-899x/743/1/012029
Subject(s) - fly ash , geopolymer , bottom ash , portland cement , materials science , curing (chemistry) , sodium hydroxide , compressive strength , coal combustion products , coal , building material , composite material , waste management , metallurgy , cement , chemical engineering , engineering
Geopolymers are amorphous to semi-crystalline with excellent physical and and mechanical properties. It has been used to become a potential binder to Ordinary Portland Cement (OPC) in certain applications due to its lower emission of carbon dioxide gases and low energy consumption sustainability criteria. Bottom Ash (BA) is one of the main industrial by-products and it is produced at the bottom of the furnace during the coal combustion process in electricity generation. The application of BA as a sustainable construction material in the building industry plays an important role in order to decrease the volume of residual waste and conserving existing natural fine aggregates. The objectives for this study is to study the effect of fly ash to bottom ash ratio and to determine the optimum ratio of fly ash to bottom ash geopolymer for pavement brick application. The chemical composition and morphology of geopolymer reinforcement was analysed by using X-ray Fluorescence and Scanning Electron Microscope. The molarity of the Sodium Hydroxide solution is fixed at 12M. The parameter used in this study are different weight percentage of fly ash geopolymer 0 wt%, 10 wt%, 20 wt%, 30 wt% and 40 wt%. The solid to liquid ratios for this study is 2.0. The curing temperature of this study is 80°C and the curing time is 24 hours. 100% of bottom ash geopolymer is used as a control variable for this study.