z-logo
open-access-imgOpen Access
The Effect of Precursors Concentration on the Structural Properties of MoS2Nanosheet-Microsphere Synthesized Via Hydrothermal Route
Author(s) -
I. S. Waskito,
Budhi Kurniawan,
Muhamad Ikhlasul Amal,
M. Hanifuddin
Publication year - 2019
Publication title -
iop conference series. materials science and engineering
Language(s) - English
Resource type - Journals
eISSN - 1757-899X
pISSN - 1757-8981
DOI - 10.1088/1757-899x/546/4/042048
Subject(s) - nanosheet , crystallinity , materials science , scanning electron microscope , particle size , hydrothermal circulation , chemical engineering , hydrothermal synthesis , autoclave , particle (ecology) , morphology (biology) , nuclear chemistry , nanotechnology , composite material , chemistry , metallurgy , engineering , oceanography , geology , biology , genetics
MoS 2 nanosheet-microsphere was successfully synthesized via hydrothermal route by applying precursor of ammonium heptamolybdate and thiourea. The precursor concentration was varied of 0.25 M, 0.5 M, 1.0 M and 1.5 M. The crystal structure, morphology and particle size of as-synthesized MoS 2 were observed as the effect of the precursors concentration. MoS 2 nanosheet-microspheres were prepared inside the hydrothermal autoclave at 200 °C for 24 hours. The X-ray diffraction (XRD) characterization result showed the structure of hexagonal 2H-MoS 2 crystals in the absence of other secondary phase. XRD characterization results also revealed that MoS 2 with a precursor concentration of 0.25 M has better crystallinity in 002 plane compared to MoS 2 synthesized with other precursor concentrations. The Scanning Electron Microscopy (SEM) observation indicated the shape of nanosheets with a thickness of several tens nanometers which were assembled to form microsphere. SEM result also showed precursor concentrations of 0.25M to 1.5M affects to the formation of nanosheet-microsphere MoS 2 particle in which along the increasing of the precursor concentration the nanosheet-microsphere particle not all well-formed. Particle Size Analyzer result showed the average particle size decreased and the average specific surface area increased with increasing precursor concentration.