Effect of annealing hold time on thickness and optical properties of barium titanate solar cell material
Author(s) -
Yoyok Cahyono,
Seni Ramadhanti,
Rasmianti,
Y N K Dewi,
M. Zainul Asrori
Publication year - 2021
Publication title -
journal of physics. conference series
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.21
H-Index - 85
eISSN - 1742-6596
pISSN - 1742-6588
DOI - 10.1088/1742-6596/1816/1/012062
Subject(s) - materials science , annealing (glass) , grain size , solar cell , band gap , absorbance , barium titanate , optoelectronics , perovskite (structure) , energy conversion efficiency , microstructure , perovskite solar cell , composite material , optics , chemical engineering , ceramic , physics , engineering
The development of perovskite-based solar cells has recently attracted the attention of many researchers because the efficiency value increases rapidly in a short span of time. Third generation solar cells have the potential to achieve Shockley-Queisser Limit of 31% for single energy bandgap solar cells. Besides that, this solar cell technology is economically very promising because the manufacturing costs are cheaper. The main drawback of this solar cell is its low stability (lifetime), which is caused by degradation over its lifetime. In addition, most of the high efficiency perovskite-based solar cells still use lead (Pb), so they are not environmentally friendly. Another alternative perovskite material is required. One promising material is Barium Titanate (BaTiO 3 ). As a material for solar cells, not much research has been done. BaTiO 3 film has been successfully made, which is then given annealing treatment at temperature of 500 °C, with annealing time of 30 minutes, 60 minutes, 90 minutes, and 120 minutes. In general, increasing the annealing time increases absorbance, decreases film thickness, decreases energy bandgap, and tends to reduce grain size of film. Energy bandgap tends to decrease with the increasing grain size. The grain size of film decreases with the decreasing thickness. More in-depth characterization and analysis are needed, especially those related to microstructure analysis.