z-logo
Premium
Tensile bond strengths of hard chairside reline resins as influenced by water storage
Author(s) -
Cucci A. L. M.,
Rached R. N.,
Giampaolo E. T.,
Vergani C. E.
Publication year - 1999
Publication title -
journal of oral rehabilitation
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.991
H-Index - 93
eISSN - 1365-2842
pISSN - 0305-182X
DOI - 10.1046/j.1365-2842.1999.00428.x
Subject(s) - bond strength , acrylic resin , ultimate tensile strength , materials science , composite material , adhesive , dental bonding , dentistry , universal testing machine , medicine , layer (electronics) , coating
Due to gradual resorption of the edentulous ridge bone, removable prostheses often require denture base relines to improve fit and stability. This research evaluated the bond strength between one heat‐cured acrylic resin (Lucitone 550®) and two hard chairside reline resins, after two different periods of storage in water (50 h and 30 days). The bond strength was evaluated using a tensile test. The mode of failure, adhesive or cohesive, was also recorded. The results submitted to the Kruskal–Wallis test indicated that the highest tensile strengths were achieved with intact Lucitone 550® denture base resin in both periods of storage in water. After 50 h of storage in water, Duraliner II® reline material exhibited the highest bond strength to the denture base resin. After 30 days of storage in water, Duraliner II® reline resin demonstrated a significant reduction in adhesion, showing lower tensile bond strength than Kooliner® material. Both hard chairside reline materials failed adhesively across Lucitone 550® denture base resin, in both periods of time.