Premium
Magnetic Fe 3 O 4 @ polydopamine biopolymer: Synthesis, characterization and fabrication of promising nanocomposite
Author(s) -
Davodi Behzad,
Jahangiri Mansoor,
Ghorbani Mohsen
Publication year - 2019
Publication title -
journal of vinyl and additive technology
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.295
H-Index - 35
eISSN - 1548-0585
pISSN - 1083-5601
DOI - 10.1002/vnl.21627
Subject(s) - thermogravimetric analysis , nanocomposite , point of zero charge , materials science , superparamagnetism , fourier transform infrared spectroscopy , nanoparticle , analytical chemistry (journal) , chemical engineering , nanotechnology , nuclear chemistry , magnetization , organic chemistry , adsorption , chemistry , engineering , physics , quantum mechanics , magnetic field
In this work, Functional Fe 3 O 4 @ polydopamine nanocomposite (Fe 3 O 4 @PDA) with magnetic response and special surface area were successfully assembled utilizing the strong coordination interactions between these two versatile materials. The morphology and size, crystal structure, specific saturation magnetization, chemical structure, and thermal properties were characterized by transmission electron microscopy (TEM), X‐ray diffraction (XRD), vibration magnetometer (VSM), point of zero charge (pH pzc ), Fourier infrared (FT‐IR) and thermogravimetric analysis (TGA). The self‐polymerization of dopamine could be completed within 3 days, and Fe 3 O 4 nanoparticles were embedded into PDA polymer. TGA results showed that PDA content of nanocomposite can be up to 51.7 wt% and also showed a significant decrease in the decomposition temperature of PDA from 530 to 270°C in the presence of the Fe 3 O 4 nanoparticles. Through TGA analysis the coating thickness was estimated to be about 0.86 nm that it is well coincident with the measured values using TEM images and XRD analysis. At room temperature by vibrating sample magnetometer (VSM), Fe 3 O 4 and Fe 3 O 4 @PDA exhibit superparamagnetic behavior with a saturation moment of 57.87 and 44.7 emu/g, respectively. Furthermore, PZC value reduced for Fe 3 O 4 @PDA compared with Fe 3 O 4 nanoparticles and fell from 6.7 to 3.04. J. VINYL ADDIT. TECHNOL., 25:41–47, 2019. © 2018 Society of Plastics Engineers