z-logo
Premium
Recent advances in steel cleanliness
Author(s) -
Höfer Friedrich,
Abratis Horst,
Geck HansGünter,
Patel Pervez
Publication year - 1993
Publication title -
steel research
Language(s) - English
Resource type - Journals
eISSN - 1869-344X
pISSN - 0177-4832
DOI - 10.1002/srin.199300982
Subject(s) - tundish , metallurgy , inert , inert gas , casting , continuous casting , materials science , chemistry , composite material , organic chemistry
At Klöckner Edelstahl in Georgsmarienhütte improvements in steel cleanliness mentioned in this report were concentrated on the tundish and pouring channel. Sealing of the tundish with inert gas curbed reoxidation so that total oxygen after about 1 minute of casting was around 10 ppm, whereas this value was reached only after 25 minutes of casting in the case without inert gas sealing. Reoxidation in the pouring channel may be a danger because of the high pressure drops recorded. Therefore, stringent measures must be observed to prevent reoxidation in the tundish and the pouring channel.

This content is not available in your region!

Continue researching here.

Having issues? You can contact us here