Premium
Cold cracking behaviour of two medium‐strength steels StE 355 containing 0.10 and 0.13 % C
Author(s) -
Hoffmeister Hans,
Bretz Wolfgang,
Fischer Klaus,
Blome Bernhard
Publication year - 1984
Publication title -
archiv für das eisenhüttenwesen
Language(s) - English
Resource type - Journals
eISSN - 1869-344X
pISSN - 0003-8962
DOI - 10.1002/srin.198405303
Subject(s) - cracking , materials science , metallurgy , composite material
Three dimensional instrumented restraint cracking (IRC) tests on steel StE 355. Welding of double‐V‐joints with basic electrodes in dry or moistured state. Critical heat input for prevention of delayed cracking. Correlation with hardness values in the coarse grained HAZ. Comparison of IRC nominal fracture stresses with literature results of implant tests.