z-logo
Premium
Temperature dependent photoluminescence studies in Cs I : T l films with varying thicknesses
Author(s) -
Shinde Seema,
Singh S. G.,
Sen Shashwati,
Gadkari S. C.,
Gupta S. K.
Publication year - 2014
Publication title -
physica status solidi (b)
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.51
H-Index - 109
eISSN - 1521-3951
pISSN - 0370-1972
DOI - 10.1002/pssb.201349180
Subject(s) - photoluminescence , exciton , excitation , materials science , atmospheric temperature range , doping , silicon , activator (genetics) , analytical chemistry (journal) , photoluminescence excitation , molecular physics , atomic physics , condensed matter physics , optoelectronics , chemistry , physics , biochemistry , chromatography , quantum mechanics , meteorology , gene
Films of Tl doped CsI in the 10 nm to 3 µm thickness range were deposited on silicon substrates using the physical vapor deposition technique under vacuum conditions. The films exhibited a columnar growth behavior with a preferential orientation along 〈200〉. The photoluminescence (PL) properties of the deposited films were studied in the 77–300 K temperature range and found to be significantly different compared to the bulk CsI:Tl single crystal. In the excitation process, the unperturbed self trapped exciton (STE) excitation of the host was found to be dominant in films of lower thicknesses and direct excitation in “A” band of Tl + and STE perturbed by the Tl + gradually evolved with increasing film thickness. At low temperatures, the PL from a 1 µm thick CsI:Tl film revealed an unperturbed STE excitation at 5.9 eV with a corresponding emission around 3.7 eV that vanishes near room temperature. This suggests that the energy transfer from the host excitons to the activator site (Tl + ) is weak at low temperatures in the CsI:Tl films.