Self‐reinforced polypropylene/LCP extruded strands and their moldings
Author(s) -
Liang Y. C.,
Isayev A. I.
Publication year - 2002
Publication title -
polymer engineering and science
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.503
H-Index - 111
eISSN - 1548-2634
pISSN - 0032-3888
DOI - 10.1002/pen.11008
Subject(s) - materials science , ultimate tensile strength , composite material , maleic anhydride , polypropylene , extrusion , polymer , molding (decorative) , morphology (biology) , thermotropic crystal , polymer blend , copolymer , liquid crystalline , biology , genetics
Polypropylenes (PP) of various molecular weights were mixed with a thermotropic liquid crystal polymer (LCP) and strands were prepared by extrusion and stretching. The strands were subsequently pelletized and then injection molded at temperatures below the melting point of LCP. The mechanical properties and the morphology of the strands and injection‐molded specimens were investigated as a function of draw ratio, LCP concentration, and PP molecular weight. The results for strands show that an increase in the draw ratio, LCP concentration and matrix molecular weight in general enhance the modulus and tensile strength. However, the tensile properties of injection‐molded specimens are found to be reduced compared with those of the original strands, in particular at high LCP concentration. The morphology of LCP changes from spherical or ellipsoidal droplets to elongated fibrils in the strands as the draw ratio increases, but this aligned LCP fibrillar morphology was not transferred to the injection‐molded specimens because of the disorientation of fibrils during injection molding. Compatibilization of PP/LCP blends was also studied by using various polymers. Maleic anhydride and acrylic acid modified PPs improved the tensile properties modestly, but maleic anhydride modified EPDM reduced the tensile properties.