Non‐destructive inspection and risk assessment for the inner wall scale exfoliation of high temperature boiler tube
Author(s) -
Cui X.H.,
Liu Y.M.,
Liu X.F.,
Zheng F.P.,
Cao H.T.
Publication year - 2014
Publication title -
materials and corrosion
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.487
H-Index - 55
eISSN - 1521-4176
pISSN - 0947-5117
DOI - 10.1002/maco.201106385
Subject(s) - boiler (water heating) , materials science , tube (container) , austenite , metallurgy , composite material , engineering , waste management , microstructure
The non‐destructive inspection method of scale on the inner wall of the ferritic steel and austenitic steel of high temperature boiler tube and the application effect were introduced in our work. The risk of scale exfoliation on the inner wall was also assessed. The risk of tube burst caused by scale exfoliation and accumulation, was reduced greatly, or even avoided by means of the change or treatment of high‐risk tube confirmed by non‐destructive inspection method.