Premium
Simultaneous and Sensitive Detection of Cd(II) and Pb(II) Using a Novel Bismuth Film/Ordered Mesoporous Carbon‐molecular Wire Modified Graphite Carbon Paste Electrode
Author(s) -
Zhao Guo,
Wang Hui,
Liu Gang,
Wang Zhiqiang
Publication year - 2017
Publication title -
electroanalysis
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.574
H-Index - 128
eISSN - 1521-4109
pISSN - 1040-0397
DOI - 10.1002/elan.201600430
Subject(s) - materials science , electrode , dielectric spectroscopy , graphite , detection limit , cyclic voltammetry , bismuth , electrochemical gas sensor , analytical chemistry (journal) , anodic stripping voltammetry , electrochemistry , carbon paste electrode , mesoporous material , carbon fibers , nuclear chemistry , chemistry , metallurgy , composite material , chromatography , organic chemistry , catalysis , composite number
An electrochemical sensor for the simultaneous and sensitive detection of Cd(II) and Pb(II) is proposed on the basis of square‐wave anodic stripping voltammetry (SWASV) experiments using a novel bismuth film/ordered mesoporous carbon‐molecular wire modified graphite carbon paste electrode (Bi/OMC‐MW/GCPE). Ordered mesoporous carbon (OMC) and molecular wire (MW) (diphenylacetylene) were used as the modifier and binder, respectively. The Bi/OMC‐MW/GCPE was prepared with the addition of graphite powder, OMC and DPA at the ratio of 2 : 1 : 1. The electrochemical properties and morphology of the electrode were characterized by electrochemical impedance spectroscopy (EIS), cyclic voltammetry (CV), SWASV and scanning electron microscopy (SEM). The parameters affecting the stripping current response were investigated and optimized. The experimental results show that the prepared electrode exhibited excellent electrochemical performance, good electrical conductivity and a high stripping voltammetric response. Under optimized conditions, a linear range was achieved over a concentration range from 1.0 to 70.0 μg/L for both Cd(II) and Pb(II) metal ions, with detection limits of 0.07 μg/L for Cd(II) and 0.08 μg/L for Pb(II) (S/N=3) with the deposition time 150 s. Moreover, the sensor exhibited improved sensitivity and reproducibility compared to traditional CPEs. The fabricated electrode was then successfully used to satisfactorily detect Cd(II) and Pb(II) in real soil samples.