z-logo
Premium
Is Rhenium Diboride a Superhard Material?
Author(s) -
Qin Jiaqian,
He Duanwei,
Wang Jianghua,
Fang Leiming,
Lei Li,
Li Yongjun,
Hu Juan,
Kou Zili,
Bi Yan
Publication year - 2008
Publication title -
advanced materials
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 10.707
H-Index - 527
eISSN - 1521-4095
pISSN - 0935-9648
DOI - 10.1002/adma.200801471
Subject(s) - materials science , titanium diboride , rhenium , crystallite , composite material , metallurgy , ceramic
The average measured Hv for polycrystalline ReB 2 and Ti–B composites under different loads shows that the tendency of Hv to decrease becomes weak for large loads, and the measured hardness of ReB 2 is always lower than that of Ti–B composites. For comparison, the results from Chung et al. were inserted into the figure.