Leaching and Adsorption of Gold from Waste Printed Circuit Boards Using Iodine-Iodide Solution and Activated Carbon
Author(s) -
Batnasan Altansukh,
Kazutoshi Haga,
Ariunbolor Narankhuu,
Shigeru Kawamura,
Atsushi Shibayama
Publication year - 2016
Publication title -
engineering journal
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.246
H-Index - 20
ISSN - 0125-8281
DOI - 10.4186/ej.2016.20.4.29
Subject(s) - activated carbon , leaching (pedology) , iodide , iodine , adsorption , printed circuit board , waste management , materials science , inorganic chemistry , chemistry , metallurgy , environmental science , organic chemistry , engineering , electrical engineering , soil science , soil water
Iodine-iodide leaching and activated carbon adsorption processes for recovery of gold (Au) from waste printed circuit boards (WPCBs) were discussed in this paper. A pressure oxidative acid leaching (POAC) was carried out in an autoclave using diluted sulfuric acid (1M H 2 SO 4 ) solution in order to remove high concentrations of some base metals especially copper (Cu), aluminum (Al), iron (Fe) and zinc (Zn) due to their negative effect on gold dissolution from WPCBs. The factors affecting the performance and efficiency of the iodine-iodide leaching process; such as iodine/iodide concentration, pulp density, leaching time and leaching temperature were optimized in order to maximize the gold dissolution efficiency from the WPCBs in the iodine-iodide solution. Results indicated that the vast majority (> 99%) of gold was dissolved in the solution from the WPCBs under the optimized leaching conditions. Adsorption tests were conducted on leach liquor solutions resulting from the iodine-iodide leaching using activated carbon. Nearly 98% of gold was adsorbed from the liquor solution onto the carbon under the condition optimized in this study. The results obtained revealed that gold can be successfully recovered from this secondary resources, where the percent recovery amounts to nearly 97% for gold.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here
Accelerating Research

Address

John Eccles House
Robert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom