Abrasive Wear Characteristics of Composite Material (AA 7075 / SiC) Synthesized by Stir Casting
Author(s) -
Khansaa Dawood Salman
Publication year - 2018
Publication title -
journal of engineering
Language(s) - English
Resource type - Journals
eISSN - 2520-3339
pISSN - 1726-4073
DOI - 10.31026/j.eng.2019.01.03
Subject(s) - abrasive , materials science , microstructure , alloy , composite material , composite number , casting , aluminium , grain size , metallurgy , surface finish , indentation hardness , surface roughness , metal matrix composite
Aluminum Metal Matrix Composites (ALMMCs) was prepared by using stir casting technique for AA 7075 aluminum alloy as a matrix reinforced with SiC particles at various percentages (3, 6, 9 and 12 wt. % ) and 75µm in grain size. The prepared composite material can be used for many applications such as aerospace, automobiles and many industrial sectors. Abrasive wear test was carried out by two stages: the first stage was done by changing the emery papers at various grit sizes 180, 320, 500, and 1000µm with constant applied load 15N. While the second stage was carried out by changing the applied loads 5, 10, 15, 20 and 25N with constant emery paper at 320 µm grit size. Microstructure examination, hardness test and roughness test were performed before and after abrasive wear test. The results of this investigation showed the increasing in weight percentage of the reinforcement material leads to increase the hardness, roughness and improving the abrasive wear resistance.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here
Accelerating Research

Address

John Eccles House
Robert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom