A Comparison of Vertical Marginal Fit of Different Brands of Translucent Zirconia Crown Restorations
Author(s) -
Sattar Jabbar Abdul-Zahra Al-Hmedat
Publication year - 2017
Publication title -
journal of baghdad college of dentistry
Language(s) - English
Resource type - Journals
eISSN - 2311-5270
pISSN - 1817-1869
DOI - 10.12816/0038747
Subject(s) - crown (dentistry) , cubic zirconia , magnification , dentistry , premolar , materials science , orthodontics , significant difference , scanning electron microscope , composite material , ceramic , mathematics , molar , medicine , computer science , statistics , computer vision
Background: As the development of zirconia crown using CAD/CAM technology, the usage of full zirconia crown is gradually increased. The aim of this in-vitro study was to evaluate and contrast the vertical marginal fit of single allceramic translucent zirconia crowns constructed from different brands translucent zirconia blanks. Materials and Methods: An acrylic resin model of a left maxillary premolar was prepared all around the tooth with (1 mm) depth and 3D scanning to get fifteen STL files, then distributed into three groups (Imes-icor, Whitepeaks and Dental direct), 3D scanning and milling machine by Imes-icor CAD/CAM devise. Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid buccal, mid palatal) using a light microscope at a magnification of x100. One-way ANOVA, LSD tests were performed to determine the mean and standard deviation of the three blanks groups. Results: Statistically high significant difference (p < 0.00) was found between the groups. The marginal gap value of the groups varied Whitepeaks crowns was (105.42 ± 7) μm, which was significantly higher than the two overall mean marginal gap measured for the Imes-icor crowns (59.3 ± 4) μm and Dental direct crowns (54.5 ± 4.9) μm, the Dental direct which was lowers overall mean vertical gap measurement. Conclusions: The marginal gap values of Dental direct crowns is considerably lower than that of Whitepeaks crown, The marginal gap values of all the groups made of monolithic high translucent Y-TZP demonstrated acceptable marginal gaps values.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here
Accelerating Research

Address

John Eccles House
Robert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom