z-logo
open-access-imgOpen Access
The Sintering Mechanism of Aluminium and the Anodization of Aluminium Sintered Bodies
Author(s) -
Sadao Okuma
Publication year - 1979
Publication title -
active and passive electronic components
Language(s) - English
Resource type - Journals
eISSN - 1026-7034
pISSN - 0882-7516
DOI - 10.1155/apec.6.23
Subject(s) - anodizing , aluminium , sintering , metallurgy , materials science , mechanism (biology) , philosophy , epistemology
It has been said that aluminium is hard to sinter. This is because a hard aluminium oxide film forms naturally on exposed aluminium in air, and in the case of heat-treatment for sintering, another type of hard aluminium oxide file also forms. Thus aluminium is hard to sinter at about 600℃. The uthor has succeeded in manufacturing aluminium sintered bodies, by using a vacuum, an inactive gas or a reducible gas atmosphere for the sintering environment.The possibility of producing a satisfactory dielectric on the aluminium sintered body was also investigated. An aluminium sintered body has physical properties different from aluminium foil or plate, because it is always in the porous state.In this paper, the author presents the experimental results on aluminium sintered bodies manufactured under various conditions and the results of anodization of the sintered bodies.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here
Accelerating Research

Address

John Eccles House
Robert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom