z-logo
open-access-imgOpen Access
Initiation of shape-memory effect by inductive heating of magnetic nanoparticles in thermoplastic polymers
Author(s) -
R. Mohr,
Karl Kratz,
Thomas Weigel,
M. Lucka-Gabor,
Martin Moneke,
Andreas Lendlein
Publication year - 2006
Publication title -
proceedings of the national academy of sciences
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 5.011
H-Index - 771
eISSN - 1091-6490
pISSN - 0027-8424
DOI - 10.1073/pnas.0600079103
Subject(s) - materials science , shape memory polymer , polymer , nanoparticle , composite material , shape memory alloy , thermoplastic , magnetic nanoparticles , copolymer , magnetic field , thermal decomposition , deformation (meteorology) , nanotechnology , chemistry , organic chemistry , physics , quantum mechanics
In shape-memory polymers, changes in shape are mostly induced by heating, and exceeding a specific switching temperature, T(switch). If polymers cannot be warmed up by heat transfer using a hot liquid or gaseous medium, noncontact triggering will be required. In this article, the magnetically induced shape-memory effect of composites from magnetic nanoparticles and thermoplastic shape-memory polymers is introduced. A polyetherurethane (TFX) and a biodegradable multiblock copolymer (PDC) with poly(p-dioxanone) as hard segment and poly(epsilon-caprolactone) as soft segment were investigated as matrix component. Nanoparticles consisting of an iron(III)oxide core in a silica matrix could be processed into both polymers. A homogeneous particle distribution in TFX could be shown. Compounds have suitable elastic and thermal properties for the shape-memory functionalization. Temporary shapes of TFX compounds were obtained by elongating at increased temperature and subsequent cooling under constant stress. Cold-drawing of PDC compounds at 25 degrees C resulted in temporary fixation of the mechanical deformation by 50-60%. The shape-memory effect of both composite systems could be induced by inductive heating in an alternating magnetic field (f = 258 kHz; H = 30 kA x m(-1)). The maximum temperatures achievable by inductive heating in a specific magnetic field depend on sample geometry and nanoparticle content. Shape recovery rates of composites resulting from magnetic triggering are comparable to those obtained by increasing the environmental temperature.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here
Accelerating Research

Address

John Eccles House
Robert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom