Low Coefficient of Thermal Expansion (CTE) Nickel Base Superalloys for Interconnect Applications in Intermediate Temperature Solid Oxide Fuel Cells (SOFC)
Author(s) -
David E. Alman,
Paul D. Jablonski
Publication year - 2004
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2004/superalloys_2004_617_622
Subject(s) - materials science , superalloy , thermal expansion , interconnection , solid oxide fuel cell , oxide , fuel cells , nickel , metallurgy , optoelectronics , alloy , chemical engineering , computer science , electrode , computer network , anode , engineering , chemistry