z-logo
Premium
Effect of long‐term water immersion on the fracture toughness of denture base and reline resins
Author(s) -
Finoti Lívia Sertori,
Machado Ana Lucia,
Chaves Carolina De Andrade Lima,
Pavarina Ana Cláudia,
Vergani Carlos Eduardo
Publication year - 2012
Publication title -
gerodontology
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.7
H-Index - 54
eISSN - 1741-2358
pISSN - 0734-0664
DOI - 10.1111/j.1741-2358.2011.00573.x
Subject(s) - medicine , base (topology) , composite material , dentistry , materials science , mathematics , mathematical analysis
doi: 10.1111/j.1741‐2358.2011.00573.x
Effect of long‐term water immersion on the fracture toughness of denture base and reline resins purpose:  This study evaluated the fracture toughness (FT) of one denture base (Lucitone 550 – L) and four hard reline resins [Ufi Gel Hard (UH), Tokuyama Rebase II (TR), New Truliner (NT) and Kooliner (K)], and the effect of long‐term water storage on this property. Materials and methods:  Forty specimens (40 × 8 × 4 mm) of each material were made, and FT was assessed after polymerisation (control of reliners), after 48 ± 2 h in water at 37°C (control of denture base resin) and after storage in water at 37°C for 7, 90 or 180 days (all materials). Data (MPa.m 1/2 ) were analysed by two‐way anova and Games–Howell test ( p  = 0.05). Results:  Resin L exhibited the highest FT mean values. After 180 days of storage, FT mean values of L (3.37), UH (1.53) and K (1.20) were higher than those of the other periods. FT mean values of NT decreased from control (1.63) to 7 days (1.30) and then remained constant. FT mean values of TR (1.13) were similar in all periods of analysis. Conclusion:  The denture base resin L showed higher FT mean values than the reline resins. Long‐term water storage increased the FT of L, UH and K, reduced the FT of NT and did not influence the FT of TR.