On the Development of Cast ATI 718Plus® Alloy for Structural Gas Turbine Engine Components
Author(s) -
B. Peterson,
D. Frias,
D. Brayshaw,
R. Helmink,
S. Oppenheimer,
E. Ott,
R. Benn,
M. Uchic
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_787_794
Subject(s) - gas turbines , alloy , metallurgy , turbine , materials science , mechanical engineering , automotive engineering , engineering