Hydrogen Embrittlement of Cast Alloy 718 Effects of Homogenization, Grain Size and Delta-Phase
Author(s) -
Göran Sjöberg,
D. Cornu
Publication year - 2001
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2001/superalloys_2001_679_690
Subject(s) - materials science , alloy , hydrogen embrittlement , grain size , embrittlement , metallurgy , hydrogen , homogenization (climate) , delta , corrosion , biodiversity , ecology , chemistry , organic chemistry , engineering , biology , aerospace engineering