Fatigue Crack Growth Behaviors in Alloy 718 at High Temperature
Author(s) -
Jizhou Xie,
Zhao Shen,
Jun Ming Hou
Publication year - 1997
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1997/superalloys_1997_587_594
Subject(s) - materials science , alloy , paris' law , metallurgy , composite material , crack closure , fracture mechanics