The aim of this study was evaluate the tensile bond strength (TBS) among nine adhesive systems and one composite resin. The groups were made as follows: Single Bond/3M (G1), Etch & Prime 3.0 /Degussa (G2), Bond 1/Jeneric/Pentron (G3), Prime & Bond 2.1/Dentsply (G4), OptiBond FL/Kerr (G5), Stae/SDI (G6), Snap Bond/ Copalite-Cooley & Cooley (G7), Prime & Bond NT/Dentsply (G8), Scotchbond Multi Purpose Plus/3M (G9). The control group (G10) was made only with the composite resin (Z100/3M). One hundred specimens were made, 10 for each group. There were significant differences on TBS among groups. G3 showed the hightest TBS in comparison to other tested groups. G10 presented higher TBS than all groups.
O objetivo desta pesquisa foi investigar in vitro a resistência de união entre uma resina composta e nove sistemas adesivos dentinários. Os adesivos estudados foram assim agrupados: Single Bond/3M (G1), Etch & Prime 3.0/ Degussa (G2), Bond 1/Jeneric/Pentron (G3), Prime & Bond 2.1/Dentsply (G4), OptiBond FL/Kerr (G5), Stae/SDI (G6), Snap Bond/Copalite (G7), Prime & Bond NT/Dentsply (G 8), Scotchbond Multi Purpose Plus/3M (G9). O Grupo controle (G10). foi confeccionado somente com a resina composta (Z100/3M). Foram confeccionados 100 espécimes, 10 para cada grupo. Houve diferenças estatísticas significantes entre os grupos. O grupo 3 foi o que mostrou a mais alta resistência em comparação aos nove testados. O grupo controle (G10) apresentou a mais alta resistência entre todos os Grupos.